Chemical Blisters
 
 << Back
Description:
Non-moisture causing blisters appear where the underside of blister is glossy.

Cause:
The new paint is not chemically compatible with the existing paint surface.

Prevention:
  • Use a compatible finish coat.
  • Make sure to properly clean and prep surface.
Cure:
Remove all paint, clean, prime & top-coat.